Proceedings of the 9th International Symposium on Superalloy 718 & Derivatives: Energy, Aerospace, and Industrial Applications (The Minerals, Metals & Materials Series)
معرفی کتاب «Proceedings of the 9th International Symposium on Superalloy 718 & Derivatives: Energy, Aerospace, and Industrial Applications (The Minerals, Metals & Materials Series)» نوشتهٔ Eric Ott, Xingbo Liu, Joel Andersson, Zhongnan Bi, Kevin Bockenstedt, Ian Dempster, Jon Groh, Karl Heck, Paul Jablonski, Max Kaplan, Daisuke Nagahama, Chantal Sudbrack، منتشرشده توسط نشر Springer International Publishing : Imprint : Springer در سال 2018. این کتاب در فرمت pdf، زبان انگلیسی ارائه شده است.
This technical meeting will focus on Alloy 718 and Superalloys in this class relative to alloy and process development, production, product applications, trends and the development of advanced modeling tools. The symposium provides an opportunity for authors to present technical advancements relative to a broad spectrum of areas while assessing their impact on related fields associated with this critical alloy group. There are continuing innovations relative to these alloys as well as novel processing techniques which continue to extend applications in very challenging environments ranging from corrosion resistance in the deep sea to high-stressed space applications. Front Matter ....Pages i-xix Front Matter ....Pages 1-1 Age Hardenable Nickel-Based Alloy Developments and Research for New High Temperature Power Cycles (John P. Shingledecker, John A. Siefert)....Pages 3-22 Superalloy 718: Evolution of the Alloy from High to Low Temperature Application (Shailesh Patel, John deBarbadillo, Stephen Coryell)....Pages 23-49 Front Matter ....Pages 51-51 Alloy 718: Laser Powder Bed Additive Manufacturing for Turbine Applications (R. Kelkar, A. Andreaco, E. Ott, J. Groh)....Pages 53-68 Progress in the Processing and Understanding of Alloy 718 Fabricated Through Powder Bed Additive Manufacturing Processes (Michael M. Kirka, Alex Plotkowski, Peeyush Nandwana, Anil Chaudhary, Suresh S. Babu, Ryan R. Dehoff)....Pages 69-88 Impact of Powder Variability on the Microstructure and Mechanical Behavior of Selective Laser Melted Alloy 718 (Chantal K. Sudbrack, Bradley A. Lerch, Timothy M. Smith, Ivan E. Locci, David L. Ellis, Aaron C. Thompson et al.)....Pages 89-113 The Effect of Location and Post-treatment on the Microstructure of EBM-Built Alloy 718 (Sneha Goel, Jonas Olsson, Magnus Ahlfors, Uta Klement, Shrikant Joshi)....Pages 115-129 Front Matter ....Pages 131-131 ICME Based Additive Manufacturing of Alloy 230 Components (Suresh Sundarraj, Sion Pickard, Alonso Peralta, Anil Chaudhary, David Snyder, Jeff W. Doak et al.)....Pages 133-146 Simulation of Co-precipitation Kinetics of γ′ and γ′′ in Superalloy 718 (Fan Zhang, Weisheng Cao, Chuan Zhang, Shuanglin Chen, Jun Zhu, Duchao Lv)....Pages 147-161 Front Matter ....Pages 163-163 Performance of Wrought Superalloys in Extreme Environments (B. A. Pint)....Pages 165-178 Corrosion and Carburization Behaviour of Ni-Cr-Mo-Nb Superalloys in a High Temperature Supercritical-CO2 Environment (Sung Hwan Kim, Chaewon Kim, Gokul Obulan Subramanian, Changheui Jang)....Pages 179-192 High Performance New Ni-Base Alloy AF955 (AF955) for Oil and Gas Industry (Luca Foroni, Louis Lherbier, Carlo Malara)....Pages 193-207 Hydrogen Influence on Crack Propagation and Stress-Strain Evolution of Alloy 718 (Sergey Kolesov, Robert Badrak, Aleksey Shakhmatov)....Pages 209-218 Isothermal Oxidation Behavior of EBM-Additive Manufactured Alloy 718 (Esmaeil Sadeghimeresht, Paria Karimi, Pimin Zhang, Ru Peng, Joel Andersson, Lars Pejryd et al.)....Pages 219-240 Front Matter ....Pages 241-241 A Computational Model of the Electroslag Remelting (ESR) Process and Its Application to an Industrial Process for a Large Diameter Superalloy Ingot (Kanchan M. Kelkar, Corey J. O’Connell)....Pages 243-261 Effect of Homogenization Temperature on Microstructures of IN718C Alloy with Different Solidification Cooling Rates (Xiaofei Yuan, Fanguo Meng, Qiang Zeng, Wei Li, Shengguo Kong, Jiantao Wu et al.)....Pages 263-273 Grain Refinement on Microstructure and Mechanical Properties of IN718 Superalloy (Taiwen Huang, Ziqi Jie, Jun Zhang, Lin Liu, Hengzhi Fu)....Pages 275-286 Melt Parameters and Resulting Characteristics in Laboratory-Scale Electroslag Remelting (Martin Detrois, Paul D. Jablonski)....Pages 287-302 Production of Nitride-Free 718 by the VIM-VAR Processing Route (Ioná Macedo Leonardo, Cláudio Silva da Hora, Mariana Beatriz dos Reis Silva, Kleber Sernik)....Pages 303-315 Front Matter ....Pages 317-317 Characterization and Modeling of Deformation Mechanisms in Ni-Base Superalloy 718 (D. McAllister, D. Lv, L. Feng, H. Deutchman, A. Wessman, Y. Wang et al.)....Pages 319-338 Characterization of a Nano-scale γ′ Phase in HPT-Disk P/M Superalloy HGN300 by Small-Angle X-Ray Scattering (M. Ohnuma, T. Yoshioka, T. Ishida, J. Nishimura, M. Sato, D. Nagahama et al.)....Pages 339-351 Development of an Automated Property Simulation Tool for Direct Aged Alloy 718 Engine Disk Forgings (Martin Stockinger, Aleksandar Stanojevic, Volker Wieser, Peter Raninger)....Pages 353-367 Microstructure Dependence of Dynamic Impact Behaviour of ATI 718plus® Superalloy (G. Asala, J. Andersson, O. A. Ojo)....Pages 369-378 3D Stochastic Modelling of Microstructure Evolution During Solidification of Alloy 718 (Laurentiu Nastac)....Pages 379-387 Analysis of Microporosity-Dependent Fatigue Crack Behavior in Alloy 718 by Using Synchronic Radiation X-Ray CT and FEM (Yahui Liu, Maodong Kang, Yun Wu, Mengmeng Wang, Haiyan Gao, Jun Wang)....Pages 389-404 Characterization of the Initial Stages of Dynamic Recrystallization in ATI 718Plus® (C. Kienl, A. Casanova, O. M. D. M. Messé, C. Argyrakis, C. M. F. Rae)....Pages 405-420 Compositional Design and Mechanical Properties of INCONEL® Alloy 725 Variants (Martin Detrois, Kyle A. Rozman, Paul D. Jablonski, Jeffrey A. Hawk)....Pages 421-437 Constrained Lattice Misfit Measurement in Bulk Inconel 718 Using High Resolution Neutron Diffraction (R. Y. Zhang, Z. N. Bi, H. L. Qin, J. Zhang, A. D. Fortes, H. B. Dong)....Pages 439-448 Dependence of Creep Strength on Cooling Rate After Subsolvus Solution Treatment in Wrought Alloy 718 (Satoru Kobayashi, Chuuya Aoki, Tomonori Ueno, Masao Takeyama)....Pages 449-459 Depletion Induced Grain Growth in Alloy 751 After Long Term Aging and Its Effect on Fatigue (Mark D. Veliz)....Pages 461-476 Effect of Grain-Boundary Fe2Nb Phase on Stress-Assisted Grain-Boundary Oxidation Behavior in Novel Austenitic Heat-Resistant Steel of Fe-20Cr-35Ni-2.5Nb (Y. Sueishi, M. Takeyama, H. Tezuka)....Pages 477-487 Effect of Heat Treatment on Microstructure and Mechanical Properties of VDM Alloy 780 Premium (M. Bergner, J. Rösler, B. Gehrmann, J. Klöwer)....Pages 489-499 Effect of Homogenization on Creep of Additive Manufactured Alloy 718 (Tomoki Otsuka, Hideki Wakabayashi, Daisuke Igarashi, Achmad Ariaseta, Shinya Imano, Yuting Wang et al.)....Pages 501-513 Effects of Post-processing on Microstructure and Mechanical Properties of SLM-Processed IN-718 (Mohsen Seifi, Ayman A. Salem, Daniel P. Satko, Richard Grylls, John J. Lewandowski)....Pages 515-526 Effects of Phosphorus Addition on Creep Properties of Wrought γ′ Strengthened Ni-Based Superalloy (Y. Hasebe, M. Yoshida, E. Maeda, S. Ohsaki)....Pages 527-540 Enhanced Strength of Inconel 718 by High Rate Severe Plastic Deformation (Prabhat Chand Yadav, Shashank Shekhar)....Pages 541-552 Evaluation of the Stress-Strain State in Alloy 718 After Hydrogen Charging (S. Kolesov, E. Alekseeva)....Pages 553-563 Experimental TTT Diagram of HAYNES 282 Alloy (M. G. Fahrmann, L. M. Pike)....Pages 565-578 Influence of Residual Stresses on Ageing Precipitation Behavior of Alloy 718 (Hailong Qin, Zhongnan Bi, Ruiyao Zhang, Hongyao Yu, Guang Feng, Xia Guo et al.)....Pages 579-593 Machine Learning to Optimize Additive Manufacturing Parameters for Laser Powder Bed Fusion of Inconel 718 (Branden Kappes, Senthamilaruvi Moorthy, Dana Drake, Henry Geerlings, Aaron Stebner)....Pages 595-610 Mechanical Performance of Various INCONEL® 740/740H Alloy Compositions for Use in A-USC Castings (Kyle A. Rozman, Martin Detrois, Paul D. Jablonski, Jeffrey A. Hawk)....Pages 611-627 Microstructural Characterization and Mechanical Properties of Rene 65 Precipitates (C. M. Katsari, H. Che, D. Guye, A. Wessman, S. Yue)....Pages 629-641 Microstructure Development in Track-by-Track Melting of EBM-Manufactured Alloy 718 (Paria Karimi, Dunyong Deng, Esmaeil Sadeghimeresht, Jonas Olsson, Joakim Ålgårdh, Joel Andersson)....Pages 643-654 Modeling Tensile, Compressive, and Cyclic Response of Inconel 718 Using a Crystal Plasticity Model Incorporating the Effects of Precipitates (Marko Knezevic, Saeede Ghorbanpour)....Pages 655-668 Novel Fractgraphy of Ni-Based Alloy by SEM/EBSD Method (Keiji Kubushiro, Yutaro Ota, Yohei Sakakibara, Hitoshi Okada)....Pages 669-678 On the Effect of Alloying Additions to the Ni-Cr-Al-Nb Dual-Superlattice Gamma-Gamma Prime-Gamma Double Prime Superalloys (P. M. Mignanelli, N. G. Jones, M. C. Hardy, H. J. Stone)....Pages 679-690 Optimization of the Forging Process Window in Respect of AGG, IGG and Direct Age Effect in Alloy 718 Engine Disks (Aleksandar Stanojevic, Christian Bucher, Markus Gruber, Bernd Oberwinkler, Martin Stockinger)....Pages 691-709 Oxidation-Assisted Cracking at 650 °C in Superalloy 718 Manufactured by Laser Beam Melting: Effect of Temperature and Strain Rate (Alexandre Pancou, Eric Andrieu, Arnaud Votié)....Pages 711-733 Precipitation Behavior and Mechanism of Sigma Phase in Alloy 925 (Zhaoxia Shi, Xiaofeng Yan, Chunhua Duan)....Pages 735-748 Quantitative Texture Prediction of Epitaxial Columnar Grains in Alloy 718 Processed by Additive Manufacturing (Jian Liu, Qian Chen, Yunhao Zhao, Wei Xiong, Albert To)....Pages 749-755 Research of Twin Induced LCF Cracking the 718 Alloy Using In-Situ Observation (Lu Xudong, Du Jinhui, Deng Qun, Wang Minqing, Bi Zhongnan, Zhang Yuchun)....Pages 757-768 Shear Spinning of Nickelbased Super-Alloy 718 (Fredrik Niklasson)....Pages 769-778 Strain Controlled Low Cycle Fatigue Behavior of U720Li Disk Superalloy Above 700 °C (Fei Sun, Yuefeng Gu, Kyoko Kawagishi, Hideyuki Murakami, Yoko Yamabe-Mitarai)....Pages 779-788 Stress Relaxation Behavior Comparison of Typical Nickel-Base Superalloys for Fasteners (He Jiang, Jing Yang, Jianxin Dong, Maicang Zhang, Zhihao Yao, Xishan Xie)....Pages 789-804 Study of the Oxidation Assisted Intergranular Cracking Mechanism on a Ni-Base Superalloy (J. Milanese, E. Andrieu, J. B. Osio, J. Alexis, D. Bardel)....Pages 805-815 The Effect of Grain Size on the Dwell Fatigue Crack Growth Rate of Alloy ATI 718Plus® (Minqing Wang, Jinhui Du, Qun Deng, Xudong Lv, Chengbin Yang, Jianxin Dong)....Pages 817-828 Thermal Processing Design of Cast INCONEL® Alloy 740H for Improved Mechanical Performance (Martin Detrois, Kyle A. Rozman, Paul D. Jablonski, Jeffrey A. Hawk)....Pages 829-846 Front Matter ....Pages 847-847 A Simplified Varestraint Test for Analyzing Weldability of Fe-Ni Based Superalloys (P. Alvarez, L. Vázquez, P. M. García-Riesco, P. P. Rodríguez, A. Magaña, F. Santos)....Pages 849-865 Fracture Toughness and Fatigue Behaviour of Variably Precipitated Inconel 625/AISI 304L Welds (Sandeep Singh Sandhu, A. S. Shahi)....Pages 867-879 Pitting Behavior of Thermally Aged Inconel 625 Weld Claddings Made Using SMAW and GMAW Process (A. S. Shahi, Sandeep Singh Sandhu)....Pages 881-898 Review of Weldability of Precipitation Hardening Ni- and Fe-Ni-Based Superalloys (Joel Andersson)....Pages 899-916 The Influence of Base Metal Microstructure on Weld Cracking in Manually GTA Repair Welded Cast ATI 718Plus® (Fabian Hanning, Joel Andersson)....Pages 917-928 Varestraint Weldability Testing of ATI 718Plus®—Influence of Eta Phase (Sukhdeep Singh, William Fransson, Joel Andersson, Anssi Brederholm, Hannu Hänninen)....Pages 929-937 Front Matter ....Pages 939-939 The Case for Physical Experiments in a Digital Age (Erin McDevitt, Ramesh Minisandram, Matias Garcia-Avila)....Pages 941-956 The High-Temperature Bauschinger Effect in Alloy 718 (S. L. Semiatin, P. N. Fagin, B. Streich, R. L. Goetz, V. Venkatesh)....Pages 957-975 Influence of Temperature and Strain Rate During Rolling of René 65 Bar (Oscar R. Terrazas, Mark E. Zaun, Ramesh S. Minisandram, Michael L. Lasonde)....Pages 977-986 Microstructure Controlling of U720-Typed Superalloys to Improve a Hot and Cold Workability by Using Incoherent Gamma Prime (A. Ota, N. Ueshima, K. Oikawa, S. Imano)....Pages 987-999 Ring Rolling of IN 718 for Critical Engine Applications (M. Büscher, T. Witulski)....Pages 1001-1011 The Abnormal Dynamic Recrystallization Behavior of a Large Alloy 706 Disc (Shuo Huang, Beijiang Zhang, Wenyun Zhang, Guangpu Zhao, Zhanfu Qi)....Pages 1013-1031 Front Matter ....Pages 1033-1033 Application of Analytical Electron Microscopy and Tomographic Techniques for Metrology and 3D Imaging of Microstructural Elements in Allvac® 718PlusTM (A. Kruk, G. Cempura, S. Lech, A. M. Wusatowska-Sarnek, A. Czyrska-Filemonowicz)....Pages 1035-1050 Computed Tomography as an Alternative Method to Measure Crack Growth in Non-conventional Geometries (Adrian Loghin, Vipul Gupta, Anjali Singhal, Al Cerrone)....Pages 1051-1072 Development of New Alloy 718 with Super Machinability (Chihiro Furusho, Yuya Kousai, Mototsugu Osaki, Koichi Uno)....Pages 1073-1085 Development of Ni-Base Disk Alloy for Large-Size Gas Turbines by Improving Macrosegregation Property of Alloy 718 (T. Shibayama, J. Sato, N. Sato, T. Nonomura, E. Shimohira, T. Uehara et al.)....Pages 1087-1101 Back Matter ....Pages 1103-1118
دانلود کتاب Proceedings of the 9th International Symposium on Superalloy 718 & Derivatives: Energy, Aerospace, and Industrial Applications (The Minerals, Metals & Materials Series)